An original Arco Solar textured etch produced with a 2% KOH solution @ 80 C with additions of 100 ml isopropyl alcohol about every hour. It’s an alkali etch which produces the surface tetrahedrons.
Donated by Omnisil Inc
An original Arco Solar textured etch produced with a 2% KOH solution @ 80 C with additions of 100 ml isopropyl alcohol about every hour. It’s an alkali etch which produces the surface tetrahedrons.
Donated by Omnisil Inc
Company | Arco |
Year | 1981 |
Cell Type | Mono-crystalline, Silicon |
Location | MOSE |
Part No. | Unknown |
Primary Use | Experimental, |
Size | 100x100 mm |
Acquisition | Donated |